Thermal processing
The suitable hot working temperature of Inconel718 alloy is 1120-900℃, and the cooling method can be water quenching or other rapid cooling methods. After hot working, it should be annealed in time to ensure the best performance. The material should be heated to the upper limit of the processing temperature during hot processing. In order to ensure the plasticity during processing, the final processing temperature when the deformation reaches 20% should not be lower than 960°C.